Zytel® FE3071 NC010 | PA66 NYLON
RESIN
Regional Availability
North America, South and Central America
Processing
Injection Moulding, Film Extrusion, Profile Extrusion, Sheet
Extrusion, Other Extrusion, Coatable, Casting
Delivery form
Pellets
Product Text
Common features of Zytel® nylon resin include mechanical and
physical properties such as high mechanical strength, excellent balance of
stiffness and toughness, good high temperature performance, good electrical and
flammability properties, good abrasion and chemical resistance. In addition,
Zytel® nylon resins are available in different modified and reinforced grades
to create a wide range of products with tailored properties for specific
processes and end-uses. Zytel® nylon resin, including most flame retardant
grades, offer the ability to be coloured.
The good melt stability of Zytel® nylon resin normally
enables the recycling of properly handled production waste. If recycling is not
possible, DuPont recommends, as the preferred option, incineration with energy
recovery (-31kJ/g of base polymer) in appropriately equipped installations. For
disposal, local regulations have to be observed.
Zytel® nylon resin typically is used in demanding
applications in the automotive, furniture, domestic appliances, sporting goods
and construction industry.
Zytel® FE3071 NC010 is an intermediate viscosity polyamde 66
resin for injection moulding and extrusion.
Injection molding
PREPROCESSING
Drying recommended = Yes, if moisture content of resin
exceeds recommended level
Drying temperature = 80℃
Drying time, dehumidified dryer = 2-4 h
Processing moisture content = <0.05 %
PROCESSING
Melt temperature optimum = 290℃
Melt temperature range = 280-300℃
Mould temperature optimum = 70℃
Mould temperature range = 50-90℃
PROPERTIES
Mechanical properties
|
dry / cond
|
Unit
|
Test Standard
|
Tensile Modulus
|
3100 / -
|
MPa
|
ISO 527-1/-2
|
Yield stress
|
82 / -
|
MPa
|
ISO 527-1/-2
|
Yield strain
|
4 / -
|
%
|
ISO 527-1/-2
|
Nominal strain at break
|
35 / -
|
%
|
ISO 527-1/-2
|
Charpy notched impact strength,23℃
|
6 / -
|
kJ/m2
|
ISO 179/1eA
|
Thermal properties
|
dry / cond
|
Unit
|
Test Standard
|
Melting temperature,10℃/min
|
262 / *
|
℃
|
ISO 11357-1/-3
|
Temp. of deflection under load,1.8
MPa
|
70 / *
|
℃
|
ISO 75-1/-2
|
Temp. of deflection under load,0.45
MPa
|
200 / *
|
℃
|
ISO 75-1/-2
|
Other properties
|
dry / cond
|
Unit
|
Test Standard
|
Density
|
1140 / -
|
kg/m3
|
ISO 1183
|